ASTM A512 Cold-drawn Welded Steel Mechanical Tubes
covers cold-drawn buttweld carbon steel tubes for use as mechaninal tubing
This specification covers round,square,rectangular,and special shape mechanical tubing.
Round tube size ranges covered are outside diameters up 3 to1/2in.(88.9mm)and wall thickness from 0.035 to 0.500in.(0.89to12.70mm)
Chemical Composition Limits, %  | |||||
Grade Designation  | 
Carbon  | 
Manganese  | 
Phospho-rus,max  | 
Sulfur, max  | 
|
MT  | 
1010  | 
0.05-0.15  | 
0.3-0.6  | 
0.045  | 
|
MT  | 
1015  | 
0.10-0.20  | 
0.3-0.6  | 
0.04  | 
0.045  | 
MT X  | 
1015  | 
0.10-0.20  | 
0.6-0.9  | 
0.04  | 
0.045  | 
MT  | 
1020  | 
0.15-0.25  | 
0.3-0.6  | 
0.04  | 
0.045  | 
MT X  | 
1020  | 
0.15-0.25  | 
0.7-1.00  | 
0.04  | 
0.045  | 
Rimmed or capped steels which may be used for the above grades are characterized by a lack of uniformity in their chemical composition, and for this reason product analysis is not technologically appropriate unless misapplication is clearly indicated.
Chemical Composition Limits, %  | ||||
Grade DesignationB  | 
Carbon  | 
Manganese  | 
Phospho-rus,max  | 
Sulfur, max  | 
1008  | 
0.10 max  | 
0.50 max  | 
0.040  | 
0.045  | 
1010  | 
0.08–0.13  | 
0.30–0.60  | 
0.040  | 
0.045  | 
1012  | 
0.10–0.15  | 
0.30–0.60  | 
0.040  | 
0.045  | 
1015  | 
0.12–0.18  | 
0.30–0.60  | 
0.040  | 
0.045  | 
1016  | 
0.12–0.18  | 
0.60–0.90  | 
0.040  | 
0.045  | 
1018  | 
0.14–0.20  | 
0.60–0.90  | 
0.040  | 
0.045  | 
1019  | 
0.14–0.20  | 
0.70–1.00  | 
0.040  | 
0.045  | 
1020  | 
0.17–0.23  | 
0.30–0.60  | 
0.040  | 
0.045  | 
1021  | 
0.17–0.23  | 
0.60–0.90  | 
0.040  | 
0.045  | 
1025  | 
0.22–0.28  | 
0.30–0.60  | 
0.040  | 
0.045  | 
1026  | 
0.22–0.28  | 
0.60–0.90  | 
0.040  | 
0.045  | 
1030  | 
0.27–0.34  | 
0.60–0.90  | 
0.040  | 
0.045  | 
1035  | 
0.31–0.38  | 
0.60–0.90  | 
0.040  | 
0.045  | 
1110  | 
0.08–0.15  | 
0.30–0.60  | 
0.040  | 
0.130C  | 
1115  | 
0.13–0.20  | 
0.60–0.90  | 
0.040  | 
0.130C  | 
1117  | 
0.14–0.20  | 
1.00–1.30  | 
0.040  | 
0.130C  | 
Rimmed or capped steels which may be used for the above grades are characterized by a lack of uniformity in their chemical composition, and for this reason product analysis is not technologically appropriate unless misapplication is clearly indicated.
B Other analyses are available.
C Grades 1110, 1115 and 1117 shall contain 0.08 min % sulfur.
Element  | 
Limit, or Maximum of Specified  | 
Variation, Over Maximum Limit or Under Minimum Limit  | 
|
Range, %  | 
Under min, %  | 
Over max, %  | 
|
Carbon  | 
To 0.15, incl  | 
0.02  | 
0.03  | 
Over 01.5  | 
0.03  | 
0.04  | 
|
Manganeses  | 
To 0.60, incl  | 
0.03  | 
0.03  | 
O  | 
|||